PropertyValue
http://www.w3.org/1999/02/22-rdf-syntax-ns#type
http://www.w3.org/ns/prov#value
  • The amount of the acid formed by hydration of diphosphorus pentaoxide or the salt thereof to be used (coating amount per 1 m2 of photosensitive material) may be any desired amount corresponding to the performance such as the sensitivity or fogging and it is preferably from 0.1 mg/m2 or more and 500 mg/m2 or less, and more preferably 0.5 mg/m2 or more and 100 mg/m2 or less.
http://www.w3.org/ns/prov#wasQuotedFrom
  • google.com