| http://www.w3.org/ns/prov#value | - In fact, by a test wherein an abrasive eraser having a diameter of 5 mm was reciprocated 10 times with a stroke of 30 mm under a load of 500 g, the number of scratch marks was the minimum with the amorphous film of the present invention among the above four types of samples, as visually observed.
|