| http://www.w3.org/ns/prov#value | - Step C) can then be partly or entirely dispensed with.The above-described variants and preferred embodiments also apply to this subject matter, so that repetition of these will be dispensed with at this point.The coating after step D) has a thickness of from 2 to 3000 .mu.m, preferably from 3 to 2000 .mu.m, in particular from 5 to 1500 .mu.m.An electrode which has been coated in this way can be in
|