. . "If desired, the substrate can be vibrated or agitated such as at about 20-30 cycles with a lateral displacement of about 50-200 mils or at about 120-160 cycles with a lateral displacement of about 5 to about 25 mils to assure removal of any particles, and air blown to further assure removal therefrom of any particles remaining from the soldering mask." . .