Utilizing suitable masking a common layer 93 of a suitable material such as chromium is sputtered into the V-shaped recess 91 to a suitable thickness as for example, 300 Angstroms followed by a layer 94 of a suitable material such as gold of a suitable thickness as for example 3000 Angstroms.