stituted by an alcohol with the weight of said solvent lying between three times and twenty times the weight of the zirconium alcoholate; impregnating said aluminum membrane structure and its optional macroporous support with said zirconiferous solution in such a manner as to cause the pores of said structure to be filled with said solution; and progressively baking said impregnated structure so a