The polyols and/or disaccharide compounds can be employed in an amount of, for example, from 0.01 to 20, judiciously from 0.1 to 20 and, in particular, from 0.1 to 10 parts by weight per 100 parts by weight of chlorine-containing polymers and resins, such as PVC.