position has a depth of cure of from about 3 mm to about 6 mm, wherein the dental composition has a polymerization stress of from about 0.5 MPa to about 2 MPa, and wherein the dental composition has a shrinkage stress of from about 0.8 Mpa to about 2.2 MPa.Further disclosed herein is a method of making a dental composition, comprising forming an oligomeric resin having a photoresponsive moiety by