For example, the tungsten-containing compound is introduced to the substrate surface at a rate between about 1 sccm (standard cubic centimeters per minute) and about 400 sccm, such as between about 10 sccm and about 100 sccm, and pulsed for about 1 second or less, such as about 0.2 seconds or less.