most commonly used heat-sealingpolymer LDPE. Due to their stickiness, they also cause problems in extrusion, e.g. by their tendency to adhere to the cooling roll, requiring thus necessarily the adoption of low running speeds.WO patent specification 03/054634 mentions the stickiness of EMA, which increases as the proportion of methyl acrylate monomer in the polymer increases.