| prov:value
| - Its examples are CaF2, MgF2, NaAlF4, SiO2, ThF4, ZrO2, Nd2O3, SnO2, TiO2, CeO2, ZnS, In2O3.For forming the antireflection layer, for example, herein employable is a dry coating method such as a vacuum evaporation method, a sputtering method, a CVD method, an ion-plating method; or a wet coating method such as gravure coating method, a reverse coating method, die coating method.
|