Again, the preferred ratio of binder to grit in the coating is in the range 1:2 to 2:1 by weight, and the coating can be applied by spraying, or other suitable technique, air dried at room temperature, and then oven dried, for example at 250??? F. As before, the coating can then be suitably finished, whereupon the diamond film can be deposited.