| http://www.w3.org/ns/prov#value | - s in the range of 0.01 to 100 ??m, especially 0.1 to 10 ??m, in order to ensure the excellent transparency of the layer and the enhanced bonding strength between the layer and the transparent conductive layer. [0123] The undercoat layer can be formed by applying a coating liquid of an appropriate composition onto a polymer film with a coater such as bar coater, and curing the coated layer by ultra
|