http://www.w3.org/ns/prov#value | - To force this reaction between aluminum and polysilicon, the preferred method heats, or anneals, the integrated-circuit assembly to approximately 450??? C. in a nitrogen, forming gas, or other non-oxidizing atmosphere for approximately 60 minutes.
|