| http://www.w3.org/ns/prov#value | - A silicon carbide glue layer may be deposited in one embodiment by introducing into a plasma processing chamber an organosilicon compound at a flow rate between about 50 and about 300 sccm, and an aliphatic hydrocarbon comprising a carbon-carbon double bond or a carbon-carbon triple bond, at a flow rate between about 50 and about 500 sccm, such as between about 100 and about 500 sccm, and optional
|