| http://www.w3.org/ns/prov#value | - To the present thermosetting powder paint composition are added, as necessary, additives such as antiblocking agent, surface control agent, plasticizer, antistatic agent, pigment, filler, extender and the like; the mixture is melt-kneaded thoroughly at about 40???-130??? C. and then cooled; the resulting material is uniformly ground into appropriate particle sizes (generally about 100 mesh or less
|