| http://www.w3.org/ns/prov#value | - Furthermore, additives such as surfactant, toner and fluorescent whitening agent were added thereto and the solution was coated on a photographic base paper of about 80 g/m2 or a Tetron base film of about 0.05 mm in thickness in the same manner as in Examples 1- 4 to obtain a positive paper or positive film for diffusion transfer.
|