| http://www.w3.org/ns/prov#value | - The film thickness is adjusted so as to become a thickness, for example around 50 nm, that functions as a protective film to prevent diffusion of H2O. Next, annealing to evaporate the organic solvent containing the protective material is carried out in an oxygen atmosphere at about 400.
|