http://www.w3.org/ns/prov#value | - In order for cured products to exhibit excellent properties such as flexibility, toughness and film-forming properties, a phenoxy resin is used which preferably has an average molecular weight (weight-average molecular weight in terms of polystyrene as measured by gel permeation chromatography) of at least 10,000, more preferably at least 20,000, and still more preferably at least 30,000.
|