| http://www.w3.org/ns/prov#value | - Depending on the pulling rate, the amount of recharged material in the case of a 4 diameter crystal is 20-40 g/min.The length of the crystal so grown is only limited by the length of the furnace when complete and is, as a rule, not more than 3 m, in particular 2.50 m.
|