| http://www.w3.org/ns/prov#value | - It is also possible to form the agglomerates by selecting a wax or other binder material that has a low melting point, such as below 200??? C., preferably below 100??? C. The low melting binder material can be mixed with the other agglomerate components and the resulting mixture can than be heated and cooled to produce the agglomerates.
|