| http://www.w3.org/ns/prov#value | - Those processes are conducted until sufficient metal is deposited on the polymer film to achieve a light transmissivity less than 20 percent, preferably less than 5 percent, even more preferably less than 3 percent, such as about 2 percent or less, or even more preferably about 1 percent or less, when measured according to Japanese Industrial Standard K 7105.
|