  • As shown in Table 8 & 9, Test Composition VI exhibited better mechanical properties, such as for example higher transverse rupture strength, hardness, and ultimate tensile strength, compared to Reference Powder V when sintered at both 2050 & 2300 degrees Fahrenheit.