  • The extruded samples were pelletized and re-extruded with additional crystal clear polystyrene, SEBS rubber, glass fibers, and other additives to give a final composition of 34 weight percent polyphenylene ether, 35.5 weight percent polystyrene, 5.5 weight percent rubber, 10 weight percent glass fibers, and 15 weight percent other additives.