| http://www.w3.org/ns/prov#value | - For comparison, the same procedure was repeated except that the material used was a laminate of a white paper of 50 g/m2 and the same polyethylene film used as the second seal layer in Example 1, to obtain oxygen absorbent packages of 50???50 mm.
|