| http://www.w3.org/ns/prov#value | - In this case, one generally employs 20 to 80, particularly 30 to 70, and particularly preferred 40 to 60 parts by weight of surface-modified powder (either as such or in the form of a dispersion, e.g. prepared as above), 10 to 70, particularly 20 to 60, and particularly preferred 30 to 50 parts by weight of dispersion medium and 0.5 to 20, particularly 2 to 15, particularly preferred 5 to 10 parts
|