  • In accordance with the present invention, the foregoing and other objects and advantages are accomplished by melt mixing 100 parts by weight of an epoxy resin, and from 1 to 100 parts by weight of pellets of a modified selectively hydrogenated block copolymer comprising at least one polymeric block comprising predominantly monoalkenyl aromatic hydrocarbon monomer units and at least one polymeric b