  • In this annealing cycle, the composite material may be annealed at a suitable temperature such as approximately 180??? F. for a suitable period such as approximately ten (10) hours, then at a suitable temperature such as approximately 212??? F. to 220??? F. for a suitable period such as approximately eight (8) hours, then at a suitable temperature of approximately 225??? F. for a suitable time per