  • ning a base metal such as nickel, copper, or an alloy thereof there can be employed as the internal electrodes 8 and 9 without any problem.During sintering to obtain the dielectric ceramic, the ratio of (average grain size of dielectric ceramic product)/(average particle size of provided starting material powder), which is represented by R, is preferably about 0.90-1.2.