  • It is preferable that Cu, Ag, Au or the alloy including them as the main component, which is 1 to 10 nm in thickness, is used for the non-magnetic layer, and a Co or Co based alloy layer of 1 to 10 nm in thickness is used for the magnetization fixed layer and the antiferromagnetic film made of FeMn, IrMn, NiMn, Ni(Co)O, etc., which is 2 to 50 nm in thickness, is used for the bias film.