  • Usually, based upon 100 parts by weight of copolymer to be produced, about 50 to 1200, preferably 100 to 600 parts by weight of solvent, usually a hydrocarbon solvent such as benzene, hexane, cyclohexane; or other suitable solvents, e.g. t-butyl alcohol, etc., and about 1 to 20 parts by weight of initiator will be used.