| http://www.w3.org/ns/prov#value | - When the functional layer is an anti-reflection layer, the layer may be formed from a resin composition containing a fine powder (a fine powder of submicron level) of an inorganic compound such as silicon dioxide, silicon oxide, aluminum oxide, magnesium fluoride and gold.
|