| http://www.w3.org/ns/prov#value | - When the sum is more than 20 wt %, the crystal structure may change from a metastable tetragonal crystal to a structure that is mainly a cubic crystal so that the ceramic layer may be deteriorated significantly in strength and tenacity and lowered in the thermal cycle resistance.
|