| http://www.w3.org/ns/prov#value | - Previously it has been possible to accomplish this either by heating a tank and liner assembly to temperatures above 390 C. and maintaining pressure during heating and cooling as previously mentioned or by a modification of this technique wherein the surface to be lined is preliminarily lined with a thin coating of poly tetrafluoroethylene applied from dispersion, such as the dispersions disclosed
|