| http://www.w3.org/ns/prov#value | - Alternatively, a redox catalyst composition can be employed wherein the polymerization temperature ranges from about 25??? to about 80??? C. Exemplary redox catalyst compositions include a peroxygen compound as described hereinbefore, preferably potassium persulfate or t-butyl hydroperoxide, and a reducing component such as sodium metabisulfite or sodium formaldehyde hydrosulfite.
|