| http://www.w3.org/ns/prov#value | - The dispersions of the silanes of formula (I) can be prepared e.g. with the aid of known dispersing apparatuses, such as ultraturrax, shear-blade and shear-slit dissolvers, optionally in the presence of surfactants, at temperatures of room temperature (ca. 20??? C.) to 100??? C. Surfactants that may be mentioned are: polyethers, as for example polyethylene oxide with an average molecular weight of
|