  • The foregoing Table II and Dispersion Examples I and II employed panels coated with the primer composition shown in Primer Example I above with a primer coating weight of about 1.5 mg./sq. in., and a primer bake of about 10 minutes at 390 F. Pigments, dyes, and other materials may be added to the dispersions and primer compositions of the invention for decorative purposes and the like, without mat