  • The adhesive that is pre-mixed with the activating fluid will already be activated when delivered to the powder mixture and will adhere filler and other particles to form a solid, agglomerated structure, as described above. [0042] Within a few minutes after the activating fluid is delivered to the particulate mixture, the fluid (with adhesive dissolved or suspended therein) infiltrates the less-so