  • Then the articles, including the surface to be coated, were heated in the chamber to a coating temperature which is in a decomposition temperature range for the aluminizing precursor to be used, no greater than about 600??? F. and generally in the range of about 350???-400??? F. The coating precursor was heated to and held at a temperature below its boiling point such that the vapor pressure of th