  • The first four monomers listed can be mixed and degassed with nitrogen, after which the last ingredient, a thermal initiator, is introduced into the mixture, the mixture being introduced into the spinning tube as hereinbefore described and raising the spinning tube with the material therein to a suitable temperature such as for example 65??? C. After polymerization, the tube is cut into suitable l