| http://www.w3.org/ns/prov#value | - The conditions for the diamond powder synthesis of the present invention, such as gas pressure, carbon sources, gas composition, flow rate, etc., may be identical with those for the conventional diamond film synthesis using CVD method, except that the temperature of the substrate II is below about 477??? C., which is relatively low compared with the conventional diamond film synthesis temperature
|