  • In an aspect, after heating to the first temperature, the sacrificial binder can be present in the topcoat layer in an amount ranging from about 0% to about 5% by weight, for example from about 0.1 to about 3 wt. %, such as from about 0.5 to about 1 wt. %, relative to the total weight of the topcoat composition.