| http://www.w3.org/ns/prov#value | - These resist materials, however, are all designed for use with electron rays, and if they are exposed to ultraviolet light, such as KrF excimer laser light, there arise such problems as imperfect resolution of the bottom portion (footing) of the pattern and formation of scums and consequent transfer of such scums to the pattern during etching.
|