| http://www.w3.org/ns/prov#value | - Further, the layer adjoining the quantum well layer is formed such as to be 0.5 nm to 2 nm in thickness, and the outside layer having a tensile strain is formed such as to have band gap energy smaller than that of the layer adjoining the quantum well layer.
|