  • Furthermore, to still improve the bindability, etc., another compound such as a polyurethane, polyester or epoxy resin can also be added to the sizing solution, but to keep the polar group density in the deposit, it is preferable that the added amount of these compounds is kept at 30 wt % or less of all the deposit.