http://www.w3.org/ns/prov#value | - The results were as shown in Table 1.EXAMPLE 14-15An abrasion resistant layer-forming material of the same formula as used in Example 1 was polymerized for a varying length of time, i.e. 1 minute and 7 minutes by following the procedure of Example 12.
|