  • The outer cover, backsheet member was a stretch thermal laminate composed of a 17 g/m2 polypropylene spunbond fabric bonded to a 17.7 g/m2, co-extruded linear-low-density-polyethylene film having a 2.5% by basis weight skin layer of catalloy and ethyl vinyl acetate (available from Kimberly-Clark Corporation located in Dallas, Tex.).