| http://www.w3.org/ns/prov#value | - Device according to claim 4, characterised in that the hot melt pressure sensitive adhesive is produced from between 10 and 80% by wt., preferably 20 to 80% by wt. and especially preferably 20 to 50% by wt., polymer, between 1 and 80% by wt., preferably 1 to 60% by wt. plasticizer; between 10 and 80% by wt. preferably 15 to 60% by wt., tackifier, optionally 0.1 to 5% by wt., anti-agers and optiona
|