| http://www.w3.org/ns/prov#value | - For maximizing the higher zone D, the converter blowing must be performed in such a way that the (FeO) content in the slag is controlled to the lowestlevel as possible while the blown-off phosphorus [P] content is controlled in a range which satisfies a standard specification of the final product, thus reducing causes of the variation in the blowing conditions, such as the reblowing ratio.
|