  • However, if desired and particularly if the alloy is strip cast, the alloys may be optionally solutionized annealed at a temperature of from about 750??? to about 950??? C. for a period of from about 30 seconds to about 8 hours and, preferably, from about 1 minute to about 4 hours followed by rapid cooling, which is preferably water quenching.